logo

ZHENGZHOU SONGYU HIGH TEMPERATURE TECHNOLOGY CO.,LTD william@songyuht.com 86-0371-6289-6370

ZHENGZHOU SONGYU HIGH TEMPERATURE TECHNOLOGY CO.,LTD Company Profile
products
Home > products > Silicon Carbide Rod > ED Type Silicon Carbide Rod

ED Type Silicon Carbide Rod

Product Details

Place of Origin: China

Brand Name: SONGYU

Payment & Shipping Terms

Minimum Order Quantity: 10pcs

Price: Negotiable

Packaging Details: WOODEN CASE

Delivery Time: 15 work days

Payment Terms: T/T, Western Union

Supply Ability: 10-1000pcs

Get Best Price
Product Details
Highlight:

ed type silicon carbide rod

,

ed silicon carbide rod

,

ed silicon carbide element

Application:
High Temperature Heating Elements
Flexural Strength:
250 - 300 MPa
Thermal Shock Resistance:
Good
Chemical Resistance:
Excellent
Shape:
Rod
Compressive Strength:
2000 - 2500 MPa
Electrical Resistivity:
10^5 - 10^6 Ω·cm
Type:
ED Type
Length:
300mm - 2000mm
Diameter:
3mm - 54mm
Maximum Operating Temperature:
1600°C
Thermal Conductivity:
120 - 150 W/mK
Density:
3.1 - 3.2 G/cm3
Material:
Silicon Carbide
Application:
High Temperature Heating Elements
Flexural Strength:
250 - 300 MPa
Thermal Shock Resistance:
Good
Chemical Resistance:
Excellent
Shape:
Rod
Compressive Strength:
2000 - 2500 MPa
Electrical Resistivity:
10^5 - 10^6 Ω·cm
Type:
ED Type
Length:
300mm - 2000mm
Diameter:
3mm - 54mm
Maximum Operating Temperature:
1600°C
Thermal Conductivity:
120 - 150 W/mK
Density:
3.1 - 3.2 G/cm3
Material:
Silicon Carbide
Product Description

   ED Type Silicon Carbide Rod    instructions:

1.The phenomenon of increasing resistance over time during the use of silicon carbide rods is called aging. Aging of the rod will cause a decrease in furnace temperature
2.For normal use, the voltage can be appropriately increased or the wiring method can be changed to compensate for the furnace temperature.

3.During power transmission, the voltage should gradually increase. It is advisable to start with half of the rated voltage to prevent rapid temperature rise. Avoid overloading during power transmission.

4.Continuous use of silicon carbide rods can improve their lifespan.

5.Silicon carbon rods are hard and brittle, so special care should be taken during loading, unloading, and transportation.

6.Silicon carbon rods should be placed in a dry place to prevent the aluminum head from getting damp and deteriorating. The heated workpiece should not contain excessive moisture and should be dried in advance to avoid affecting the lifespan of the rod. If it is a new kiln or a kiln that has not been used for a long time, old rods must be used for kiln drying, and new rods should be avoided.

7.Silicon carbon rods become brittle and shorten their lifespan when used in hydrogen gas.

8.Silicon carbide rods can corrode when in contact with alkali metals, alkalis, silicates, borides, etc., so it is important to avoid contact between them and the rod body.

9.The silicon carbide rod wire clamp should be in close contact with the aluminum head at the cold end of the rod body.

10.If the silicon carbide rod is found to be broken or burnt during use, it should be replaced with a new rod in case of emergency. To avoid affecting the service life of other rods.

Application High Temperature Heating Elements
Flexural Strength 250 - 300 MPa
Thermal Shock Resistance: Good
Chemical Resistance Excellent
Shape Rod
Compressive Strength 2000 - 2500 MPa